Molykote
MOLYKOTE Specialty Lubricants & Lubrication Solutions
MOLYKOTE® is DuPont's specialty-lubricants portfolio for controlling friction, wear, sealing, release, and component movement across automotive and industrial equipment. The portfolio spans greases, oils & fluids, pastes, compounds, anti-friction coatings, and dispersions, with product technologies that include mineral oil, synthetic hydrocarbon, ester, silicone, fluorosilicone, PFPE, and solid-lubricant systems. Depending on the product, MOLYKOTE solutions support bearings, gears, chains, compressors, pumps, valves, seals, threaded connections, electric motors, sliding surfaces, and other demanding lubrication points.
As an authorized MOLYKOTE distributor, Krayden supplies specialty lubricants for equipment design, production, maintenance, and repair applications. Our team can help compare lubricant type, base chemistry, viscosity or consistency, load, speed, temperature, environmental exposure, material compatibility, and application method so customers can narrow the appropriate MOLYKOTE options for a specific operating condition.
Markets Served by MOLYKOTE
Greases
MOLYKOTE greases combine a lubricating fluid, thickener, and performance additives or solid lubricants to stay in place where a flowing oil is not practical. The portfolio spans general machinery lubrication, high-load and severe-duty service, wide-temperature applications, chemically demanding environments, and low-noise or precision-bearing duties. Selection should account for load, environment, temperature, speed, relubrication interval, base-oil chemistry, thickener system, and compatibility with nearby metals, plastics, elastomers, or process media.
Oils & Fluids
MOLYKOTE oils and fluids provide flowing lubrication for gears, gearboxes, pumps, chains, compressors, vacuum equipment, slides, and other machinery where circulation, penetration, or controlled fluid delivery is preferred over a grease. The portfolio includes mineral and synthetic base-fluid technologies. Selection should consider viscosity, operating temperature, load and speed, oxidation or corrosion exposure, equipment design, material compatibility, and any process-specific requirements.
Pastes
MOLYKOTE pastes are greaselike lubricants with a high concentration of solid lubricants for assembly, running-in, anti-seize, and heavily loaded metal contact. They are commonly considered for threaded connections, press fits, splines, gears, and other slow-moving or startup contacts where the carrier oil may be displaced but a solid lubricating film is still needed. Product selection should consider substrate metallurgy, load, temperature, corrosion exposure, required friction behavior, and assembly or disassembly requirements.
Compounds
MOLYKOTE compounds are greaselike silicone-based materials used where lubrication and sealing, release, electrical insulation, moisture resistance, or compatibility with rubber and plastics may be required. The category extends beyond release compounds to include valve and seal lubrication, O-ring assembly, dielectric moisture barriers, noncuring sealing functions, and selected plastic or elastomer lubrication duties. Confirm product-specific compatibility and any regulatory or process requirements for the intended application.
Anti-Friction Coatings
MOLYKOTE anti-friction coatings are bonded dry-film lubricants containing solid lubricants dispersed in resin and solvent systems. After application and curing, they form a thin lubricating film on the component surface and are used where a clean, dry lubricant is preferred, where dust or contamination makes wet lubrication undesirable, or where relubrication access is limited. Coating choice depends on substrate, surface preparation, application method, cure requirements, film thickness, load, motion, and service environment.
Dispersions
MOLYKOTE dispersions suspend finely divided solid lubricants in a liquid carrier so the lubricant can be applied by liquid methods, including automatic dispensing where appropriate. They are used for dry-film lubrication of sliding contacts, lubrication of chains, conveyors and bearings in demanding temperature conditions, selected cutting or sewing operations, release applications, and other specialty processes. Selection should consider carrier chemistry, evaporation or residue behavior, application equipment, surface material, required film, temperature, and process compatibility.
Talk to our Experts
Whether you are comparing a grease, oil, paste, compound, coating, or dispersion, Krayden can help narrow MOLYKOTE options around the actual lubrication point. Our team can support product comparison, application requirements, load-speed-temperature review, material compatibility, environmental exposure, and practical application or maintenance considerations.
MOLYKOTE Quick Reference
126 products

MOLYKOTE HI-VAC SILICONE BASED HIGH VACUUM GREASE
- Low-Volatility Silicone Grease
- Less Than 0.5% Bleed
- Seals and Lubricates Vacuum and Pressure Systems

MOLYKOTE 112
- Up to 232 deg C Service
- Oil, Acid, and Alkali Resistance
- Low-Volatility Joint Sealing

MOLYKOTE BG20
- 45 to 180 deg C Service Range
- 2,400 N Four-Ball Weld Load
- Manual or Automated Dispensing

MOLYKOTE G-1033
- FDA 21 CFR 178.3570 Compliance
- 3,922 N Four-Ball Weld Load
- Clean, White Color

MOLYKOTE L-1668FM
- ISO Vg 68 Mineral-Oil
- Low Vapor Pressure
- Carries NSF H1 Certification

MOLYKOTE G-1023
- Steel/GFRP Friction Control
- -45 to 120 deg C Service
- Automatic Dispensing Compatible

DUROPTIX OE-6370
- 1:1 Optical Encapsulant Mixing
- 100% Transparent Optical Protection
- 240-Minute 150 deg C Cure

MOLYKOTE 1122
- High-Viscosity Lubricant Formulation
- Robust High-Pressure Resistance and Wear Protection
- High-Temperature Lubrication Protection

MOLYKOTE BG-555
- Low-Noise Bearing Grease
- Water-Washout and Corrosion Resistance
- -40 to 150 deg C Service Range

MOLYKOTE G-1067
- Low-Friction Plastic-Compatible PAO Grease
- 50 to 120 deg C Service Range
- Automotive Lubrication Applications

MOLYKOTE LONGTERM 2 PLUS
- 3,800 N Four-Ball Weld Load
- Heavily Loaded Metal-to-Metal Components Protection
- 25 to 110 deg C Service Range

MOLYKOTE G2008
- High-Speed Gear Lubrication
- 30 cSt Synthetic Base Oil
- -40 to 130 deg C Service

DUROPTIX OE-6550
- 1:1 Controlled Mixing
- High Optical Transmittance
- High Refractive Index

MOLYKOTE 3099
- Water-Repellent High-Voltage Insulator Coating
- 800-Minute ASTM D2303 Arc Resistance
- Hand, Pad, Brush, or Spray Renewal

MOLYKOTE BR-2
- MoS2/Graphite Lithium Grease
- High-Load Moderate/High-Speed Lubrication
- Long-Term Industrial Lubrication

MOLYKOTE G-1502FM
- Oil and Water Resistance
- FDA 21 CFR 178.3570 Compliance
- 40 to 149 deg C Service Range

MOLYKOTE M-77
- Up to 400 deg C Service
- Silicone Carrier Oil
- Selected Metal, Plastic, Rubber, and Elastomer Contacts

MOLYKOTE G684OZTUBES
- Plastic Gear Friction Control
- 75 mm2/s Base Oil
- Brush-to-Central System Application

ECCOSORB AN-77
- Carbon Loaded, Multilayer Absorber
- Broadband Free Space Absorber
- Low-Weight RF Absorber

MOLYKOTE 316
- Effective, Heat-Stable Anti-Stick Silicone Film
- FDA 21 CFR 175.300 Compliance
- Oxidative Breakdown Resistance

MOLYKOTE CU-7439
- Up to 650 deg C Service
- High-Adhesion Copper Paste
- Nondestructive Thread-Disassembly Support

MOLYKOTE G-3000
- Dual-Mass-Flywheel High-Shear Grease
- -40 to 180 deg C Service Range
- 2,200 N Four-Ball Weld Load

MOLYKOTE P37
- -30 to 1400 deg C Threaded-Connection Lubrication
- 5,500 N Four-Ball Weld Load
- Graphite/Zirconium-Dioxide High-Purity Paste

MOLYKOTE P-1042
- 9,000 N Weld Load
- Water-Emulsion Washout Resistance
- High-Tack Metal Surface Adhesion

MOLYKOTE 3179
- Dilatant Rheological Behavior
- Non-Slumping Static-Flow Resistance
- Novelty/Educational Toy-Market Use

MOLYKOTE D-10-GBL
- 15 to 20 um Dry Film
- -40 to 340 deg C Service Range
- 5,500 N Falex Load

MOLYKOTE G-3407
- -40 to 200 deg C Service Range
- Brake-Caliper Guide-Pin Lubrication
- 120-Hour No-Rust Test Result

MOLYKOTE P-40
- Metal-Free Lubrication Paste
- Assembly and Continuous Lubrication
- -40 to 121 deg C Paste Service

MOLYKOTE P-1900
- 3,200 N Weld Load
- Controlled 0.10 Bolt Friction
- -30 to 300 deg C Service

MOLYKOTE 33
- NLGI 2 Silicone Grease
- Water-Resistant Light-Load Lubrication
- 73 to 180 deg C Service Range

MOLYKOTE D-321
- 5-Minute Cure Cycle
- 180 to 450 deg C Service Range
- 12,500 N Falex Load

MOLYKOTE G-4500FM
- 40 to 150 deg C Service Range
- 18 kg Four-Ball Weld Load
- NLGI 2 PAO/Aluminum-Complex Grease

MOLYKOTE PA-744
- 10 to 20 um Screen-Printed Film
- High-Wear High-Load Dry Lubrication
- -75 to 300 deg C Service Range

MOLYKOTE P-3700
- High-Purity Solid-Lubricant Paste
- 3,000 N Weld Load
- Controlled M12 Fastener Friction

MOLYKOTE 3400A
- 30-Minute 200 deg C Heat Cure
- High-Load Dry-Film Wear Resistance
- 500-Hour Red-Rust Resistance

MOLYKOTE D-708
- 700-Hour Cure Cycle
- 60 to 240 deg C Service Range
- 60-Minute 180 deg C Cure

MOLYKOTE G-4501
- FDA 21 CFR 178.3570 Compliance
- Lower-Consistency (NLGI 1) PAO Synthetic Grease
- 40 to 150 deg C Service Range

MOLYKOTE PG54
- Long-Term Lubrication for Metal-to-Plastic
- 50 to 180 deg C Service Range
- Silicone Base Oil

MOLYKOTE P-74
- Metal-Free Anti-Seize Formulation
- 4,800 N Weld Load
- Controlled M12 Fastener Friction

MOLYKOTE 3452
- Multi-Solvent Chemical Resistance
- Defined 8-Hour Exposure Testing
- 400 kg Four-Ball Weld Load

MOLYKOTE D-7409
- Heat-Curing Dry-Film Lubricant
- High-Load Wear-Resistant Dry-Film Lubrication
- Solvent and Oil Resistance

MOLYKOTE G-4700
- Extreme-Load Bearing Lubrication
- PAO Synthetic Base Oil and Lithium Complex Thickener
- Industrial Plastic/Elastomer Compatibility

MOLYKOTE TP-42
- 3,000 N Four-Ball Weld Load
- Water-Resistant Grease Lubrication
- Stick-Slip, Galling, and Corrosion Protection

MOLYKOTE 4
- 54 to 200 deg C Service Range
- 3 ohm-cm Volume Resistivity
- Flowable Controlled Placement

MOLYKOTE D-96
- Transparent Water-Based PTFE Dry Film
- 100,000-Cycle No-Noise Pairing Result
- -40 to 150 deg C Service Range

MOLYKOTE G-5008
- 350 V/mil Dielectric Strength
- 2.0% Bleed at 204 deg C
- NLGI 2-3 Silicone/PTFE Grease

MOLYKOTE YM103
- PAO/PTFE Lubrication for Plastic-on-Plastic
- 45 to 150 deg C Service Range
- Automotive Lubrication Applications

MOLYKOTE 3451 Chemical Resistant Bearing Grease
- Fluorosilicone Grease Formulation
- 40 to 450 deg F Service Range
- 340 kg Four-Ball Weld Load

MOLYKOTE 41
- Silicone Oil Base and Carbon Black Thickener
- 20 to 290 deg C Service Range
- Water and Oxidation Resistance

MOLYKOTE DX
- 4,800 N Four-Ball Weld Load
- 0.10 Press-Fit Friction Coefficient
- -25 to 125 deg C Service Range

MOLYKOTE G-5042
- Effective Purple Silicone Grease
- Siloxane Base Oil and Lithium Soap Thickener
- Long-Term Silicone-Grease Lubrication

MOLYKOTE Z-POWDER
- 98% MoS2 Solid Lubricant
- 185 to 400 deg C Service Range
- 0.048 Coefficient of Friction

MOLYKOTE 7 RELEASE COMPOUND
- 40 to 204 deg C Service Range
- Release, Lubrication, Sealing, and Protection
- 0.8% Evaporation at 200 deg C

MOLYKOTE 44
- -40 to 200 deg C Service Range
- 2.5% Bleed at 150 deg C
- NLGI 2-3 Silicone Grease

MOLYKOTE EM-30L
- -45 to 150 deg C Service Range
- 3,730 N Four-Ball Weld Load
- 0.4% Evaporation at 99 deg C

MOLYKOTE GN
- Mineral-Oil Solid-Lubricant Assembly Paste
- 0.08 Press-Fit Friction Coefficient
- 2,800 N Four-Ball Weld Load

MOLYKOTE D-321R AN-FR
- Room-Temperature Application Cure
- Dry Film Lubricant Formulation
- 180 to 450 deg C Service Range

MOLYKOTE 5
- Nonconductive, Water-Repellent Silicone Paste
- 54 to 232 deg C Service Range
- Metal and Plastic Compatibility

MOLYKOTE EM-50L
- Broad Plastic Compatibility
- 100% Silicone-Free PAO Grease
- Low-Seepage Long-Service Lubrication

MOLYKOTE HP-300
- Fully Fluorinated PFPE/PTFE Lubrication
- 65 to 250 deg C Service Range
- 3,300 N Four-Ball Weld Load

LAIRD LS-30
- Compliant Polyurethane Foam Format
- RF Isolation and Insertion Loss
- Cavity Resonance Suppression

MOLYKOTE EM-D110 GREASE
- Compatible with Most Plastics
- High-Viscosity PAO Oil
- Silicone-Free Lubrication Formulation

LAIRD ECCOSORB GDS
- Thin Conformable Construction
- High-Frequency RF Attenuation

LAIRD TPUTTY 502FG2
- 3.0 W/(m K) Thermal Interface
- Ultra-Soft 14 Shore 00 Material
- Thermal Interface Material

MOLYKOTE 55
- Silicone Base Oil and Lithium Soap Thickener
- Heat-Stable Oxidation-Resistant Grease
- D4/D5/D6 Cyclic-Siloxane Compliance

MOLYKOTE E-PASTE
- 560 kg Four-Ball OK Load
- ABS, Polycarbonate, Nylon, Polyacetal Compatibility
- -50 to 150 deg C Service Range

MOLYKOTE HP-870
- Fully Fluorinated Formulation
- -20 to 250 deg C Service Range
- Chemical-Resistant PFPE/PTFE Grease

LAIRD MF-117
- Machinable RF Component Stock
- 2.8 to 119 dB/cm Attenuation
- Sheets, Rods and Bars

MOLYKOTE G-2008 Synthetic Tool Gear Grease
- Fully Synthetic PAO-Based Grease with Lithium Thickener
- Manual or Automated Dispensing
- Sub-0.55 mm Four-Ball Wear

LAIRD JCP-PP9
- 60+ GHz Injection-Moldable Absorber
- 76 to 81 GHz Automotive Radar Use
- Polypropylene-Like Mechanical Integration

LAIRD VY-81
- 80 to 90 dB EMI/RF Shielding
- Non-Hardening High-Tack Shielding Compound
- Conventional Caulking-Equipment Application

MOLYKOTE 557
- Clear Nonstaining Wax-Like Film
- 0.07 Coefficient of Friction
- Federal Meat/Poultry Program Authorization

MOLYKOTE G-0010
- Polyurea-Thickened Mineral-Oil Grease
- Above 260 deg C Dropping Point
- Corrosion-Preventive Bearing Grease

MOLYKOTE L-1268
- Fully Synthetic ISO Vg 68 PAO Lubrication
- 54 deg C Pour Point
- Longer Oil-Drain Intervals

LAIRD PP-4
- 1.06 Low-Loss Dielectric Constant
- 0.0001 Loss Tangent
- Heat-Sealable Closed-Cell Foam

MOLYKOTE G-68 Plastic Gear Grease
- Good Compatibility with Most Plastics
- 0.014 Coefficient of Friction
- Water-Resistant Grease Lubrication

LAIRD LS-26
- High-Loss Microwave Absorption
- Low-Density Urethane Foam
- Very Flexible Absorber Foam

MOLYKOTE 1000
- No Intentional PFAS, Lead, or Nickel
- -30 to 650 deg C Service Range
- Consistent Friction and High Load Capacity

MOLYKOTE 7400
- Water-Based MoS2/Graphite Dry-Film Lubricant
- High Load-Carrying Capacity
- Air-Curing Lubricant Coating

MOLYKOTE G-0050
- FDA 21 CFR 178.3570 Compliance
- 3,922 N Four-Ball Weld Load
- Clean, White Color

MOLYKOTE L13
- Adjusts the Application Viscosity
- Compatible Cleaning Solvent
- Defined Range of Molykote Coatings

LAIRD RFLB/SS6M
- Adhesive-Backed 0.51 mm Sheet
- 10 MHz to 4 GHz Control
- Greater Than 50 dB/cm Attenuation

MOLYKOTE G-N METAL ASSEMBLY PASTE
- Heavy-Duty Assembly Paste
- 0.08 Coefficient of Friction
- Metal Interfaces Protection

LAIRD MCS/SS6M
- 800 MHz to 6 GHz Absorption
- Low-Outgassing Silicone Construction
- Flexible Sheet with Optional PSA

MOLYKOTE 106
- Heat-Curing Dry Film Lubricant
- High-Load Coating Application
- 70 to 250 deg C Service Range

MOLYKOTE 7415
- Molykote D-7405, D-7409, and D-7620 Anti-Friction Coatings
- Low Evaporation Rate
- PTFE- and PFAS-Free Formulation

MOLYKOTE G-0052
- FDA 21 CFR 178.3570 Compliance
- 6,080 N Four-Ball Weld Load
- Water-Resistant Grease Lubrication

MOLYKOTE L-1468 FM
- ISO VG 68 PAO Chain Oil
- Freezer-Chain Anti-Wear Lubrication
- NSF H1 Registration

MOLYKOTE BG-20
- DN 750,000 High-Speed Operation
- Medium-to-Heavy Load Lubrication
- -45 to 180 deg C Service

LAIRD TPUTTY 403
- 2.3 W/(m K) One-Part Putty
- 0.05 mm Minimum Bondline
- ASTM E595 0.05% TML/0.02% CVCM

LAIRD TPUTTY SF560
- 5.6 W/m-K Non-Silicone Putty
- 60 g/min Cartridge Flow
- Low-Fogging Reworkable Interface

LAIRD TPCM7125
- 0.125 mm Phase-Change Film
- 7.5 W/m-K Bulk Conductivity
- 25 Micrometer Minimum Bondline

LAIRD TPCM780SP
- Screen-Printable Non-Silicone Paste
- 5.4 W/m-K Dry-State Conductivity
- 25 Micrometer Minimum Bondline

LAIRD TPCM5200
- 0.200 mm Phase-Change Film
- 5.3 W/m-K Bulk Conductivity
- 25 Micrometer Minimum Bondline

LAIRD SNL60RXP
- 100 dB 200 MHz to 10 GHz Shielding
- 1-Hour Room-Temperature Handling
- -50 to 125 deg C Service Range

LAIRD TFLEX 3130
- 3.25 mm Tflex 300 Gap Filler
- Greater Than 50% Deflection at 50 psi
- 1.2 W/(m K) Thermal Conductivity

LAIRD TFLEX 300
- Over 50% Deflection at 50 psi
- 1.2 W/(m K) Thermal Conductivity
- 0.50 to 5.08 mm Thickness Range

LAIRD TFLEX 360
- 1.50 mm Gap-Filling Solution
- 50% Deflection at 50 psi
- 1.2 W/(m K) Thermal Interface

LAIRD TFLEX 640
- 1.02 mm Thickness of Tflex 600 Series
- 3.0 W/(m K) Thermal Interface
- Naturally Tacky Surfaces

LAIRD TFLEX 6150
- 3.75 mm Thickness of Tflex 600 Series
- 3.0 W/(m K) Thermal Interface
- Naturally Tacky Surfaces

LAIRD TFLEX 680
- 2.03 mm Thickness of Tflex 600 Series
- 3.0 W/(m K) Thermal Interface
- Naturally Tacky Pad Surfaces

LAIRD TFLEX 660
- 1.50 mm Medium-Gap of Tflex 600 Series
- 3.0 W/(m K) Thermal Interface
- Easy Assembly and Placement with Naturally Tacky

LAIRD TFLEX HD90500
- 7.5 W/(m K) Thermal Interface
- Compliant Silicone Gap Filler
- Naturally Tacky Construction

LAIRD TFLEX HD91000
- 1.00 mm Controlled-Compression Pad
- 7.5 W/mK Thermal Conductivity
- 0.20 C-in2/W at 10 psi

LAIRD TFLEX HD93500
- 7.5 W/(m K) Thermal Interface
- Compliant Silicone Gap Filler
- Naturally Tacky Construction

LAIRD TGON 805
- 0.13 mm Flexible Graphite Interface
- 5 W/(m K) Through-Plane Conductivity
- 0.07 deg C in^2/W Thermal Resistance


LAIRD TFLEX 6110
- 3 W/mK Thermal Conductivity
- Greater Than 90% Recovery
- Naturally Tacky Adhesive-Free Placement

LAIRD TFLEX 320H
- Dry Preformed Interface Pad
- No Mixing or Dispensing
- Controlled-Compression Gap Filling

LAIRD TFLEX 3200
- Low-Pressure Compliant Gap Filling
- Tgard Dielectric Handling Layer
- Reusable Low-Compression-Set Pad

LAIRD TFLEX SF10.0.50
- 0.50 mm Thin-Gap Format
- 10.2 W/m-K Thermal Conductivity
- Non-Silicone Electrical Insulation

LAIRD TFLEX SF10
- 10 W/m-K Non-Silicone Interface
- Low-Pressure Thermal Contact
- 0.3 to 5.0 mm Sheet Range

LAIRD TFLEX HP34
- 34 W/m-K Bulk Conductivity
- Low Contact Resistance Under Pressure
- Non-Silicone Aligned-Graphite Construction

LAIRD TFLEX HD92000
- 2.00 mm High-Deflection Interface
- 7.5 W/mK Heat Transfer
- 82% Deflection at 50 psi

LAIRD TFLEX HD93000
- 3.00 mm High-Deflection Pad
- 7.5 W/mK Thermal Conductivity
- Low-Outgassing Silicone Interface

LAIRD TPUTTY 506
- No-Cure Single-Part Putty
- 3.5 W/m-K Thermal Conductivity
- Low-Pressure Uneven-Gap Filling

LAIRD TPLI2200
- 5.08 mm Large-Gap Pad
- A0 Adhesive-Free Surface
- 6.0 W/m-K Insulating Interface

LAIRD CFS-8480
- Broad RF Absorption Capability
- Flexible Castable Processing
- Elevated-Temperature Electrical Performance

LAIRD CR-110
- Above 26 GHz Absorption Range
- 100:16.5 Controlled Mixing
- Below 180 deg C Service Temperature

LAIRD CR-114
- 10 to 14 GHz Absorption Range
- 100:6.5 Controlled Mixing
- Below 180 deg C Service Temperature

LAIRD CR-116
- 6 to 12 GHz Absorption Range
- 100:4.3 Controlled Mixing
- Below 180 deg C Service Temperature

LAIRD CR-117
- 100:3.2 Part A:B Mixing
- 4 to 8 GHz Grade Range
- ECCOSORB MF-117 Cured Equivalence

LAIRD CR-124
- Below 5 GHz Absorption Range
- 100:2.6 Controlled Mixing
- Up to 150 deg C Service Temperature

LAIRD CRS-117
- Flexible RTV Silicone Microwave Absorber
- 100:1.18 Controlled Mixing
- 0.9 W/(m K) Thermal Conductivity

LAIRD CRS-124
- Flexible RTV Silicone Microwave Absorber
- 100:1.00 Controlled Mixing
- 1.0 W/(m K) Thermal Conductivity

LAIRD CRS-124CRS-124
- Custom Cast Microwave Loads
- Above-1-GHz RF Attenuation
- Impact-Resistant Silicone Elastomer